Tensile Strength, Yield 710 MPa

@Strain 0.200 %,
Temperature 650 °C
103000 psi

@Strain 0.200 %,
Temperature 1200 °F
Precipitation Hardened prior to test
Special Metals NIMONIC® Alloy 80A
A nickel-chromium alloy similar to NIMONIC alloy 75 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good corrosion and oxidation resistance and high tensile a..
Tensile Strength, Yield 710 MPa

@Strain 0.200 %
103000 psi

@Strain 0.200 %
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Aged 732°C (1350°F)/4hr/AC
Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t..