Polymer Property : Tensile Strength, Yield = 66.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 66.7 MPa

@Thickness 3.20 mm
9670 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUMID HI1102A(W) PA6, High Impact
Feature: Injection Molding, PA6, High ImpactApplication: H/Lamp Screw MountingCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical
Tensile Strength, Yield 66.7 MPa

@Thickness 3.20 mm
9670 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOY SG5009F PC/ABS
Description: Injection Molding, PC/ABS, High Gloss, Scratch Resistance, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC & Monitor housing)CAS: 103598-77-2 and 181028-79-5Information prov..
Tensile Strength, Yield 66.7 MPa

@Thickness 3.20 mm
9670 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOY SG5009FA PC/ABS/PMMA, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High Gloss, Anti-scratchApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 9011-14-7 and 181028-79-5Informatio..
Tensile Strength, Yield 66.7 MPa

@Thickness 3.20 mm
9670 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical 82TR SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical
Tensile Strength, Yield 66.7 MPa
9670 psi
ASTM D638
IRPC Polimaxx Polene 1111NX GA6 Polypropylene Compound
CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER WITH 30% GLASS FIBRE REINFORCED HIGH IMPACT STRENGTH, HIGH MECHANICAL STRENGTH, HIGH STIFFNESS LOW SHRINKAGEAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ..
Tensile Strength, Yield 66.7 MPa
9670 psi
ASTM D638
Samyang Trirex® 3022A Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Tensile Strength, Yield 66.7 MPa
9670 psi
ASTM D638
Samyang Trirex® 3022L1 Polycarbonate, Lens Grade
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Tensile Strength, Yield 66.7 MPa
9670 psi
ASTM D638
Samyang Trirex® 3025N1 Polycarbonate, Flame Retardant
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..