IRPC Polimaxx Polene 1111NX GA6 Polypropylene Compound

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene 1111NX GA6 Polypropylene Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER WITH 30% GLASS FIBRE REINFORCED HIGH IMPACT STRENGTH, HIGH MECHANICAL STRENGTH, HIGH STIFFNESS LOW SHRINKAGEAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength, Yield 66.7 MPa
9670 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Yield Strength 82.4 MPa
11900 psi
ASTM D790
Flexural Modulus 8.50 GPa
1230 ksi
ASTM D790
Izod Impact, Notched 0.539 J/cm

@Temperature 23.0 °C
1.01 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 161 °C
322 °F
ASTM D648