Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 6385 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.02 MPa
6385 psi
ASTM D-638
Axiall 9190 Rigid PVC, Molding
Georgia Gulf 9190 was developed to aid compliance with source reduction initiatives especially when low temperature impact strength is a concern. It has superior properties, which in most cases wil..
Copyright © lookpolymers.com All Rights Reserved