Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 44.02 MPa | 6385 psi | ASTM D-638 |
Axiall 9190 Rigid PVC, Molding Georgia Gulf 9190 was developed to aid compliance with source reduction initiatives especially when low temperature impact strength is a concern. It has superior properties, which in most cases wil.. |