Tensile Strength, Yield 298 - 436 MPa

@Strain 0.200 %,
Thickness 2.50 mm
43200 - 63200 psi

@Strain 0.200 %,
Thickness 0.0984 in
Cold rolled + annealed sheet
AK Steel 41003 Ferritic Stainless steel
AK Steel 41003 is an economical steel that provides excellent weldability, toughness and fabricating characteristics. This alloy is an excellent choice for applications such as tubing and sheet for..