Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 298 MPa @Temperature 22.0 °C |
43200 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® HPC 1200 Unsaturated Polyester UP HPC 1200 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc.. |
|||
Tensile Strength, Yield | 298 MPa @Temperature 190 °C |
43200 psi @Temperature 374 °F |
Laminate property; Open Hole Tension; Conditioning: 14 days Water 158°F |
Hexcel® HexFlow® RTM651 One-part Modified BMI Resin HexFlow® RTM651 is a one-component modified bismaleimide for resin transfer molding (RTM). Upon heating to 212-248°F, the resin will become a low viscosity homogeneous liquid that has a long pot-l.. |
|||
Tensile Strength, Yield | 298 MPa | 43200 psi | Forging (Hot Forged and Heat Treated) |
CMW® 3 Copper Alloy CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre.. |
|||
Tensile Strength, Yield | 298 - 436 MPa @Strain 0.200 %, Thickness 2.50 mm |
43200 - 63200 psi @Strain 0.200 %, Thickness 0.0984 in |
Cold rolled + annealed sheet |
AK Steel 41003 Ferritic Stainless steel AK Steel 41003 is an economical steel that provides excellent weldability, toughness and fabricating characteristics. This alloy is an excellent choice for applications such as tubing and sheet for.. |