AK Steel 41003 Ferritic Stainless steel

Category Metal , Ferrous Metal , Ferritic , Stainless Steel , T 400 Series Stainless Steel
Manufacturer AK Steel
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AK Steel 41003 Ferritic Stainless steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AK Steel 41003 is an economical steel that provides excellent weldability, toughness and fabricating characteristics. This alloy is an excellent choice for applications such as tubing and sheet for bus frames, coal hopper cars, street sweepers, chutes, storage tanks, ISO shipping container frames and other equipment requiring low life-cycle costs.Information provided by AK Steel
Mechanical Properties Metric English Comments
Hardness, Rockwell B 81
81
Typical
75 - 94

@Thickness 2.50 mm
75 - 94

@Thickness 0.0984 in
Cold rolled + annealed sheet
Hardness, Rockwell C <= 20
<= 20
Specification
Tensile Strength, Ultimate 513 MPa
74400 psi
Typical
461 - 603 MPa

@Thickness 2.50 mm
66900 - 87500 psi

@Thickness 0.0984 in
Cold rolled + annealed sheet
Tensile Strength, Yield 346 MPa
50200 psi
Typical
298 - 436 MPa

@Strain 0.200 %,
Thickness 2.50 mm
43200 - 63200 psi

@Strain 0.200 %,
Thickness 0.0984 in
Cold rolled + annealed sheet
Elongation at Break 26 %
26 %
Typical
18 - 36 %
18 - 36 %
in 2 inches (Cold rolled + annealed sheet nominally 2.5 mm thick)
Charpy Impact, Notched 135 J/cm²

@Thickness 2.50 mm
642 ft-lb/in²

@Thickness 0.0984 in
Transverse [Cold rolled + Annealed + Pickled, sheet]
205 J/cm²

@Thickness 2.50 mm
976 ft-lb/in²

@Thickness 0.0984 in
Longitudinal [Cold rolled + Annealed + Pickled, sheet]
103 J/cm²

@Thickness 2.50 mm,
Temperature -30.0 °C
490 ft-lb/in²

@Thickness 0.0984 in,
Temperature -22.0 °F
Transverse [Cold rolled + Annealed + Pickled, sheet]
192 J/cm²

@Thickness 2.50 mm,
Temperature -30.0 °C
914 ft-lb/in²

@Thickness 0.0984 in,
Temperature -22.0 °F
Longitudinal [Cold rolled + Annealed + Pickled, sheet]
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 10.5 - 12.5 %
10.5 - 12.5 %
Iron, Fe >= 83.37 %
>= 83.37 %
As Remainder
Manganese, Mn <= 1.5 %
<= 1.5 %
Nickel, Ni <= 1.5 %
<= 1.5 %
Nitrogen, N <= 0.030 %
<= 0.030 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %