Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 14.5 - 59.0 MPa | 2100 - 8560 psi | Average value: 33.1 MPa Grade Count:48 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Tensile Strength, Yield | 20.0 - 59.0 MPa | 2900 - 8560 psi | Average value: 44.9 MPa Grade Count:54 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |