Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.96 MPa | 575 psi | at 200%, no post cure- press cured for 5 minutes; ASTM D412 |
Multibase C6-560 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.96 MPa | 575 psi | AVG Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 5433 Nitrile Rubber General purpose Nitrile; Low water swellInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 3.96 MPa | 575 psi | ASTM D412 |
Teknor Apex TEKBOND® 6700-45 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 3.96 MPa @Strain 300 % |
575 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® IT 38-074 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTransparentApplications:Hot Runner MoldingFDA (Food Contact)Teething ring & pacifierMulti-PurposeMarket:Consumer GoodsProcessing Method:I.. |