Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
ASTM D2240
Tensile Strength, Yield 3.96 MPa
575 psi
ASTM D412
Elongation at Break 400 %
400 %
ASTM D412