Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.92 MPa
569 psi
ASTM D412
Polymax® Maxelast® A9840 TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Tensile Strength, Yield 3.92 MPa
569 psi
at 300% elongation; ASTM D412
Lubrizol Estane® T460A Thermoplastic Polyurethane
Type: Estane® T460A is a Shore 66A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b..
Tensile Strength, Yield 3.92 MPa
569 psi
at 100% elongation, maximum
Dow Corning SILASTIC® 37087-V SILICONE RUBBER NATURAL
70 Durometer, peroxide cured, low compression set Silicone Rubber CompoundInformation provided by Dow Corning
Tensile Strength, Yield 3.92 MPa
569 psi
200%, post cured- 4 hours at 177°C; ASTM D412
Multibase C6-550 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 3.92 MPa
569 psi
at 200%, post cured- 2 hours at 177°C; ASTM D412
Multibase C6-550 Dow-Corning Class VI Elastomer
Information provided by Multibase