Polymer Property : Tensile Strength, Yield = 560 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.86 MPa
560 psi
at 200%, post cured- 2 hours at 200°C; ASTM D412
Multibase SILASTIC® Q7-4840 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase
Tensile Strength, Yield 3.86 MPa
560 psi
@50% Elongation; ASTM D1414
Greene Tweed FLUORAZ® 797 Fluoroelastomer, FEPM
Greene, Tweed`s Fluoraz® functions effortlessly in a variety of challenging process environments. Fluoraz performs well in aggressive chemicals where ultrapure materials are not required. Known f..
Tensile Strength, Yield 3.86 MPa
560 psi
200%, post cured- 8 hours at 177°C; ASTM D412
Multibase C6-250 VAROX DBPH Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 3.86 MPa
560 psi
at 200%, molded-without post cure; ASTM D412
Multibase C6-265 VAROX DBPH Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 3.86 MPa
560 psi
100%; ASTM D412
Teknor Apex APEX® 3201-65 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling..
Tensile Strength, Yield 3.86 MPa
560 psi
100%; ASTM D412
Teknor Apex APEX® 3300-60 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Food Service Applications, General Purpose, Me..
Tensile Strength, Yield 3.86 MPa
560 psi
100%; ASTM D412
Teknor Apex APEX® 3311-60 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To..
Tensile Strength, Yield 3.86 MPa
560 psi
100%; ASTM D412
Teknor Apex APEX® 3200-60 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
Tensile Strength, Yield 3.86 MPa
560 psi
ASTM D412
Teknor Apex UNIPRENE® 7100-55 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 3.86 MPa
560 psi
500 mm/min (20 in./min); ASTM-D638 Type IV Specimen
Westlake EMAC® Plus SP1501 20% EMA Copolymer
Westlake EMAC� Plus SP1501 is a 20% EMA copolymer designed for extrusion coating, compounding, and blending where low viscosity, flexibility, and strength are important. SP1501 provides excelle..
Tensile Strength, Yield 3.86 MPa
560 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® IT304 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerTranslucentNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First Choic..