Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.86 MPa | 560 psi | at 200%, post cured- 2 hours at 200°C; ASTM D412 |
Multibase SILASTIC® Q7-4840 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tensile Strength, Yield | 3.86 MPa | 560 psi | @50% Elongation; ASTM D1414 |
Greene Tweed FLUORAZ® 797 Fluoroelastomer, FEPM Greene, Tweed`s Fluoraz® functions effortlessly in a variety of challenging process environments. Fluoraz performs well in aggressive chemicals where ultrapure materials are not required. Known f.. |
|||
Tensile Strength, Yield | 3.86 MPa | 560 psi | 200%, post cured- 8 hours at 177°C; ASTM D412 |
Multibase C6-250 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.86 MPa | 560 psi | at 200%, molded-without post cure; ASTM D412 |
Multibase C6-265 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.86 MPa | 560 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3201-65 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 3.86 MPa | 560 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3300-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Food Service Applications, General Purpose, Me.. |
|||
Tensile Strength, Yield | 3.86 MPa | 560 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3311-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 3.86 MPa | 560 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3200-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 3.86 MPa | 560 psi | ASTM D412 |
Teknor Apex UNIPRENE® 7100-55 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 3.86 MPa | 560 psi | 500 mm/min (20 in./min); ASTM-D638 Type IV Specimen |
Westlake EMAC® Plus SP1501 20% EMA Copolymer Westlake EMAC� Plus SP1501 is a 20% EMA copolymer designed for extrusion coating, compounding, and blending where low viscosity, flexibility, and strength are important. SP1501 provides excelle.. |
|||
Tensile Strength, Yield | 3.86 MPa | 560 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® IT304 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTranslucentNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First Choic.. |