Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.3 MPa

@Temperature 23.0 °C
4970 psi

@Temperature 73.4 °F
ASTM D638
Ineos H01H-00 Polypropylene Homopolymer
This is a low flow rate homopolymer designed for extrusion or injection molding. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Applic..
Tensile Strength, Yield 34.3 MPa

@Temperature 23.0 °C
4970 psi

@Temperature 73.4 °F
ASTM D638
Ineos H04G-00 Polypropylene Homopolymer
This is a controlled rheology general purpose homopolymer polypropylene. This grade is designed to meet the processing and physical property requirements of film and profile extrusion applications...
Tensile Strength, Yield 34.3 MPa
4970 psi
ASTM D638
Lotte Chemical Titan TITANPRO® PM383 Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Tensile Strength, Yield 34.3 MPa
4970 psi
ASTM D638
Lotte Chemical Titan TITANPRO® PM803 Polypropylene homopolymer
Titanpro® PM803 is a high flow and also a controlled rheology grade. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (..
Tensile Strength, Yield 34.3 MPa
4970 psi
82% Ret.
UBE UBESTA® 3030U Nylon 12 (After Fuel C for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Tensile Strength, Yield 34.3 MPa
4970 psi
ASTM D638
Westlake Plastics Propylux® 290 Polypropylene, Heat Stabilized
Through process improvement and advanced engineering, Westlake Plastics introduces the next generation of heat-stabilized polypropylene. Propylux 290 is produced from a FDA approved homopolymer res..
Tensile Strength, Yield 34.3 MPa
4970 psi
ASTM D638
Westlake Plastics Propylux® HS2 Polypropylene for Medical Applications, Heat Stabilized
Through process improvement and advanced engineering, Westlake Plastics introduces the next generation of heat-stabilized polypropylene. Propylux HS2 is produced from a FDA and USP Class VI approve..
Tensile Strength, Yield 34.3 MPa
4970 psi
82% Ret.
UBE UBESTA® 3030U Nylon 12 (After Methanol for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..