Lotte Chemical Titan TITANPRO® PM383 Polypropylene homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Lotte Chemical Titan Holding Sdn. Bhd. (Former Titan Chemicals)
Trade Name TITANPRO®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANPRO® PM383 Polypropylene homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 177.1520(b). In summary, this resin meets the FDA criteria covering safe use of polyolefin articles and component of articles intended for food contact use.Applications: Oriented film for food and garment packaging, adhesive tape, lamination, photo album, pearlized film, etc.Advantages: Exceptional cleanliness and purity. Good stiffness, high clarity and gloss. Low die build up and extended die life.Fabrication: Equipment - standard BOPP machines. Techniques - standard processing. Information provided by Titan ChemicalsCAS# 9003-07-0
Physical Properties Metric English Comments
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Water Absorption 0.020 %
0.020 %
after 24 hrs; ASTM D570
Base Resin Melt Index 2.9 g/10 min

@Temperature 230 °C
2.9 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785A
Tensile Strength, Yield 34.3 MPa
4970 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790B
Izod Impact, Notched 0.529 J/cm
0.991 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648