Mechanical Properties Metric English Comments
Tensile Strength, Yield 10.3 - 31.0 MPa
1500 - 4500 psi
ASTM D638
Alcoa KAMA 3000 High Impact Polystyrene (HIPS)  (discontinued **)
CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableMono-layer an..
Tensile Strength, Yield 13.0 - 31.0 MPa
1890 - 4500 psi
Average value: 22.3 MPa Grade Count:52
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Tensile Strength, Yield 17.9 - 31.0 MPa
2600 - 4500 psi
Average value: 25.9 MPa Grade Count:15
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is ..
Tensile Strength, Yield 13.8 - 31.0 MPa
2000 - 4500 psi
Average value: 19.7 MPa Grade Count:16
Overview of materials for Medium Density Polyethylene (MDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max..
Tensile Strength, Yield 16.5 - 31.0 MPa
2390 - 4500 psi
Average value: 23.3 MPa Grade Count:116
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max..
Tensile Strength, Yield 15.2 - 31.0 MPa
2200 - 4500 psi
ASTM D638
Alcoa KAMA 3200 Prime High Impact Polystyrene  (discontinued **)
CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone trea..