Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 10.3 - 31.0 MPa | 1500 - 4500 psi | ASTM D638 |
Alcoa KAMA 3000 High Impact Polystyrene (HIPS)
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableMono-layer an.. |
|||
Tensile Strength, Yield | 13.0 - 31.0 MPa | 1890 - 4500 psi | Average value: 22.3 MPa Grade Count:52 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Tensile Strength, Yield | 17.9 - 31.0 MPa | 2600 - 4500 psi | Average value: 25.9 MPa Grade Count:15 |
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is .. |
|||
Tensile Strength, Yield | 13.8 - 31.0 MPa | 2000 - 4500 psi | Average value: 19.7 MPa Grade Count:16 |
Overview of materials for Medium Density Polyethylene (MDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Yield | 16.5 - 31.0 MPa | 2390 - 4500 psi | Average value: 23.3 MPa Grade Count:116 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Yield | 15.2 - 31.0 MPa | 2200 - 4500 psi | ASTM D638 |
Alcoa KAMA 3200 Prime High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone trea.. |