Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 255 - 300 MPa | 37000 - 43500 psi | With 0% cold work |
OMG Americas GlidCop® AL-15 Dispersion Strengthened Copper GlidCop® AL-15 is copper that is dispersion strengthened with 0.3 wt% ultrafine particles of aluminum oxide. It is produced using an internal oxidation powder metallurgy process whereby aluminum o.. |
|||
Tensile Strength, Yield | 260 - 300 MPa | 37700 - 43500 psi | |
ArcelorMittal 260 BH Bake hardening steel, Cold rolled Available in the following: uncoated (HC260B), electroglavanized (HC260B+ZE) and Extragal®/Galvannealed (HC260BD+Z)Description: The composition and processing of these steels are designed to promot.. |
|||
Tensile Strength, Yield | 260 - 300 MPa | 37700 - 43500 psi | |
ArcelorMittal IF 260 High strength IF steel, Cold rolled Available in the following: uncoated (HC260Y), electroglavanized (HC260Y+ZE) and Extragal®/Galvannealed (HX260YD+Z/+ZF)Description: These steels were designed to provide an excellent combination of.. |
|||
Tensile Strength, Yield | 140 - 300 MPa | 20300 - 43500 psi | |
ArcelorMittal 52+AS Aluminized steel Use: Average drawingInformation provided by ArcelorMittal |