Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 25.0 - 30.0 MPa | 3630 - 4350 psi | ISO.527 DN.53455 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Tensile Strength, Yield | 25.0 - 30.0 MPa | 3630 - 4350 psi | ISO.527 DN.53455 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Tensile Strength, Yield | 20.0 - 30.0 MPa | 2900 - 4350 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer
(discontinued **) Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i.. |
|||
Tensile Strength, Yield | 6.89476 - 30.0 MPa @Temperature -30.0 - 70.0 °C |
1000.00 - 4350 psi @Temperature -22.0 - 158 °F |
Average value: 20.6 MPa Grade Count:1 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |
|||
Tensile Strength, Yield | 20.0 - 30.0 MPa | 2900 - 4350 psi | Average value: 27.0 MPa Grade Count:7 |
Overview of materials for Polymethylpentene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr.. |