Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.12 MPa | 597 psi | at 200%, post cured- 2 hours at 177°C |
Multibase SILASTIC® Q7-4780 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 4.12 MPa | 598 psi | crosshead speed 20 in./min; ASTM D638 |
Dow AFFINITY™ SM 1300G Polyolefin Plastomer (POP) AFFINITY™ SM 1300G is an ethylene alpha-olefin resin for Injection Molding is produced via INSITE™ Technology from Dow Plastics. The resin offers excellent performance in durable injection molded.. |
|||
Tensile Strength, Yield | 4.12 MPa | 598 psi | 200%, post cured- 8 hours at 177°C; ASTM D412 |
Multibase C6-550 Dow-Corning Class VI Elastomer Information provided by Multibase |