Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 26.2001 - 125 MPa @Temperature -40.0 - 120 °C |
3800.01 - 18100 psi @Temperature -40.0 - 248 °F |
Average value: 74.9 MPa Grade Count:2 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |