Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 330 MPa
>= 47900 psi
MetalTek Nitronic® 40 Austenitic Stainless Steel
Produced under license of ARMCO Advanced Materials Corp. Information provided by MetalTek
Tensile Strength, Yield 330 MPa
47900 psi
Haynes Hastelloy® W alloy as a weld filler, base metal Type 304 Stainless steel 12.7 mm plate weldments
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica..
Tensile Strength, Yield 330 MPa

@Strain 0.200 %,
Temperature 540 °C
47900 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield 330 MPa

@Strain 0.200 %,
Temperature 650 °C
47900 psi

@Strain 0.200 %,
Temperature 1200 °F
Haynes 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield 330 MPa

@Strain 0.200 %,
Temperature 205 °C
47900 psi

@Strain 0.200 %,
Temperature 401 °F
Haynes Hastelloy® B-3® alloy, 6.3 mm plate
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Tensile Strength, Yield 330 MPa

@Strain 0.200 %
47900 psi

@Strain 0.200 %
Annealed prior to test
Special Metals BRIGHTRAY® Alloy C Electrical Resistance Alloy
A nickel-chromium electrical-resistance alloy for use at operating temperatures up to 2100°F (1150°C). It contains rare-earth additions for increased oxidation resistance, especially under co..
Tensile Strength, Yield 330 MPa

@Strain 0.200 %,
Temperature 550 °C
47900 psi

@Strain 0.200 %,
Temperature 1020 °F
Solution Annealed prior to test
Special Metals INCONEL® Alloy 601
A nickel-chromium alloy with an addition of aluminum for outstanding resistance to oxidation and other forms of high-temperature corrosion. It also has high mechanical properties at elevated temper..
Tensile Strength, Yield 330 MPa
47900 psi
SSAB Tunnplat Domex® 014 BOR Rolled Boron Steel
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron ..
Tensile Strength, Yield 330 - 410 MPa
47900 - 59500 psi
ArcelorMittal Dual Phase 600 Very high strength steel, Cold Rolled Steel
Available in the following: HCT780X (uncoated), HCT780X+ZE (electrogalvanized) and HCT780X+Z/ZF (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength a..
Tensile Strength, Yield 330 - 460 MPa
47900 - 66700 psi
ArcelorMittal Dual Phase 600 Very high strength steel, Hot Rolled Steel
Available in the following: HCT580X (uncoated)Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martens..