MetalTek Nitronic® 40 Austenitic Stainless Steel

Category Metal , Ferrous Metal , Austenitic , Stainless Steel , Cast Stainless Steel
Manufacturer MetalTek
Trade Name Nitronic®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek Nitronic® 40 Austenitic Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Produced under license of ARMCO Advanced Materials Corp. Information provided by MetalTek
Mechanical Properties Metric English Comments
Hardness, Brinell 185
185
Tensile Strength, Ultimate >= 620 MPa
>= 89900 psi
Tensile Strength, Yield >= 330 MPa
>= 47900 psi
Elongation at Break >= 35 %
>= 35 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.080 %
<= 0.080 %
Chromium, Cr 19 - 21.5 %
19 - 21.5 %
Iron, Fe 59.52 - 67.35 %
59.52 - 67.35 %
As Balance
Manganese, Mn 8.0 - 10 %
8.0 - 10 %
Nickel, Ni 5.5 - 7.5 %
5.5 - 7.5 %
Nitrogen, N 0.15 - 0.40 %
0.15 - 0.40 %
Silicon, Si <= 1.0 %
<= 1.0 %
Descriptive Properties Value Comments
Heat Treatment Sol. Anneal