Polymer Property : Tensile Strength, Yield = 305000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2100 MPa
305000 psi
when tempered at 350°F
Carpenter Vega® Alloy Tool Steel (Air-Tough) (AISI A6)
Vega die steel combines the deep hardening and minimum size change characteristics of air-hardening steels with the simplicity of low temperature heat treatment possible in many oil-hardening steels..