Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2100 MPa | 305000 psi | when tempered at 350°F |
Carpenter Vega® Alloy Tool Steel (Air-Tough) (AISI A6) Vega die steel combines the deep hardening and minimum size change characteristics of air-hardening steels with the simplicity of low temperature heat treatment possible in many oil-hardening steels.. |