Material Notes:
Vega die steel combines the deep hardening and minimum size change characteristics of air-hardening steels with the simplicity of low temperature heat treatment possible in many oil-hardening steels. It is available as a DeCarb-Free product. DCF bars have been cold finished in the mill, eliminating the need for bar bark removal.Applications: Large blanking dies, Large forming dies, Trimming dies, Notching dies, Feed fingers, Heavy duty punches, Coining dies, Retaining rings, Rim rolls, Master hubs, Shear blades, Precision tools, Spindles, Bending tools, Mandrels, Stripper plates, Plastic moldsInformation provided by Carpenter Technology Corporation.Vega® is a registered trademark of Carpenter Technology Corporation.
Physical Properties Metric English Comments
Specific Gravity 7.85 g/cc
7.85 g/cc
Mechanical Properties Metric English Comments
Hardness, Rockwell C 48 - 49
48 - 49
Tempered at 1200°F
61 - 62
61 - 62
As hardened
Tensile Strength, Ultimate 2350 MPa
341000 psi
when tempered at 350°F
Tensile Strength, Yield 2100 MPa
305000 psi
when tempered at 350°F
Elongation at Break 1.0 %
1.0 %
when tempered at 350°F
Reduction of Area 2.0 %
2.0 %
when tempered at 350°F
Modulus of Elasticity 200 GPa
29000 ksi
Izod Impact Unnotched 155 J
114 ft-lb
when tempered at 350°F
Charpy Impact 1.00 J
0.738 ft-lb
V-Notch, when tempered at 350°F
Charpy Impact, Unnotched 130 J

@Treatment Temp. 177 °C
95.9 ft-lb

@Treatment Temp. 350 °F
tempered at 350°F
Abrasion 73.8
73.8
loss in mm<sup>3</sup>, As-Hardened; ASTM G65
130.7
130.7
loss in mm<sup>3</sup>, Tempered at 1100°F; ASTM G65
Thermal Properties Metric English Comments
CTE, linear 11.8 µm/m-°C

@Temperature 20.0 - 100 °C
6.56 µin/in-°F

@Temperature 68.0 - 212 °F
13.7 µm/m-°C

@Temperature 20.0 - 400 °C
7.61 µin/in-°F

@Temperature 68.0 - 752 °F
14.7 µm/m-°C

@Temperature 20.0 - 700 °C
8.17 µin/in-°F

@Temperature 68.0 - 1290 °F
Component Elements Properties Metric English Comments
Carbon, C 0.70 %
0.70 %
Chromium, Cr 1.0 %
1.0 %
Iron, Fe 94.65 %
94.65 %
As Balance
Manganese, Mn 2.0 %
2.0 %
Molybdenum, Mo 1.35 %
1.35 %
Silicon, Si 0.30 %
0.30 %
Users viewing this material also viewed the following: