Polymer Property : Tensile Strength, Yield = 26100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.0 - 180 MPa
8410 - 26100 psi
Average value: 125 MPa Grade Count:49
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Tensile Strength, Yield 140 - 180 MPa
20300 - 26100 psi
ArcelorMittal 05 High formability steel for drawing, Cold rolled
Available in the following: uncoated (DC05) and electroglavanized (DC05+ZE) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These product..
Tensile Strength, Yield 140 - 180 MPa
20300 - 26100 psi
ArcelorMittal 56 High formability steel for drawing, Cold rolled
Available in the following: Extragal®/Galvannealed (DX56D +Z/+ZF)Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used..
Tensile Strength, Yield 120 - 180 MPa
17400 - 26100 psi
ArcelorMittal 56+AS Aluminized steel
Use: Extra-deep drawingInformation provided by ArcelorMittal