Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 14.0 - 17.0 MPa | 2030 - 2470 psi | 50 mm/min; ISO/R 527 |
Okulen® 1000 PE-UHMW, Green Black OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Tensile Strength, Yield | 14.0 - 17.0 MPa | 2030 - 2470 psi | 50 mm/min; ISO/R 527 |
Okulen® 1000 PE-UHMW, Multi-color OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Tensile Strength, Yield | 16.0 - 17.0 MPa | 2320 - 2470 psi | 50mm/min; ASTM D638-64T |
Micropol Microlin ML53 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |