Mechanical Properties Metric English Comments
Tensile Strength, Yield 163 MPa
23600 psi
ASTM D638
Solvay Specialty Polymers Kadel® E-1130 Polyketone  (discontinued **)
High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, plus superior chemical r..
Tensile Strength, Yield 163 MPa
23600 psi
Type I, 5 mm/min; ASTM D638
LNP ULTEM® EXCP0096 Polyetherimide, 30% Carbon Fiber Reinforcement, 10% PTFE Lubricant  (discontinued **)
Features: Lubricated, Electrically Conductive, Good Wear Resistance, High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This dat..
Tensile Strength, Yield 163 MPa
23600 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP RX06480 PA 66
LNP LUBRICOMP* RX06480 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% Lubricants. Added feature of this material is: Wear Resistant.
Tensile Strength, Yield 163 MPa
23600 psi
ASTM D638
Techmer ES Luriblend® PA6/6 GF30 TL5 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Frict..
Tensile Strength, Yield 163 MPa
23600 psi
Type I, 5 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp RF006PS PA 66
LNP* Thermocomp* RF-1006 EP HS is based on Nylon 6/6 containing Glass Fiber. Characteristics of this grade include Exceptional Processing and Heat Stabilizer.This data was supplied by SABIC-IP for ..
Tensile Strength, Yield 163 MPa
23600 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON OE004AE PPS - Branched
LNP STAT-KON* OE004AE is a compound based on PPS - Branched resin containing 20% Carbon Fiber. Added features of this material are: Easy Molding, Electrically Conductive.
Tensile Strength, Yield 163 MPa
23600 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Verton RV006ESV_GY7E071 PA 66
Preliminary Data for 30% long glass fiber, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region.