Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 21.6 - 23.5 MPa | 3130 - 3410 psi | ASTM D1708 |
Polimersan Plastics POLITEF® (PTFE) with 15% Glass As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Tensile Strength, Yield | 21.6 - 23.5 MPa | 3130 - 3410 psi | ASTM D1708 |
Polimersan Plastics POLITEF® (PTFE) with 15% Glass As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Tensile Strength, Yield | 16.0 - 23.5 MPa | 2320 - 3410 psi | Average value: 19.2 MPa Grade Count:6 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |