Polymer Property : Tensile Strength, Yield = 21.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.7 MPa
3150 psi
ASTM D638
M. Holland Company CP510 Polypropylene Copolymer
Additives: Heat Stabilizer, Nucleating AgentsFeatures: High Flow, High Impact Resistance, Heat Stabilizer, NucleatedUses: Construction Applications, Lawn and Garden EquipmentApprovals: FDA 21 CFR 17..
Tensile Strength, Yield 21.7 MPa
3150 psi
Elastic; ASTM D638
Multibase Multi-Flex® D 5500 TPO Thermoplastic Polyolefin Elastomer
Forms: PelletsProcessing Methods:Blow MoldingInformation provided by Multibase
Tensile Strength, Yield 21.7 MPa
3150 psi
ASTM D638
LyondellBasell Petrothene® LR590001 High Density Polyethylene
ApplicationsPETROTHENE LR590001 is designed as primary insulation for telephone singles. LR590001 is a high density resin designed for low shrinkback after extrusion. Antioxidant has been added to e..
Tensile Strength, Yield 21.7 MPa
3150 psi
ASTM D638
LyondellBasell Petrothene® LR590005 High Density Polyethylene
ApplicationsPETROTHENE LR 5900-05 is a high density, high molecular weight resin designed for primary insulation for electronic cables. This resin exhibits low shrinkback after extrusion, contains ..
Tensile Strength, Yield 21.7 MPa
3150 psi
ASTM D412
Teknor Apex APEX® 3301-90 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To..
Tensile Strength, Yield 21.7 MPa
3150 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 80 PHR Mistron Vapor Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tensile Strength, Yield 21.7 MPa
3150 psi
ASTM D638
Washington Penn Homopolymer Polypropylene 40% Calcium Carbonate Filled
Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa..
Tensile Strength, Yield 21.7 MPa
3150 psi
ASTM D638
Clariant Renol PPSP0006HW Polypropylene Homopolymer, Heavy Weight Compound
Data provided by Clariant Masterbatches
Tensile Strength, Yield 21.7 MPa
3150 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 80 PHR Mistron Vapor Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tensile Strength, Yield 21.7 MPa
3150 psi
ASTM D-638
Axiall 1851 Clear 7002 Flexible PVC
Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation ..