Material Notes:
Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.23 - 1.27 g/cc
1.23 - 1.27 g/cc
ASTM D-792
Melt Flow 22.38 g/10 min

@Load 23.9 kg,
Temperature 175 °C
22.38 g/10 min

@Load 52.7 lb,
Temperature 347 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 88
82 - 88
delayed; ASTM D-2240
Tensile Strength, Yield 21.7 MPa
3150 psi
ASTM D-638
Elongation at Yield 345 %
345 %
ASTM D-638
100% Modulus 0.01327 GPa
1.925 ksi
ASTM D-638
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 179 °C
355 °F