Mechanical Properties Metric English Comments
Tensile Strength, Yield 67.6 - 141 MPa
9800 - 20500 psi
Average value: 98.2 MPa Grade Count:17
Overview of materials for ABS/Polyester Alloy + GF
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro..
Tensile Strength, Yield 11.7 - 141 MPa
1700 - 20500 psi
Average value: 42.0 MPa Grade Count:90
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Tensile Strength, Yield 26.0 - 141 MPa
3770 - 20500 psi
Average value: 71.0 MPa Grade Count:5
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..