Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 67.6 MPa | 9800 psi | ASTM D638 |
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 67.6 MPa | 9800 psi | ASTM D638 |
Polymer Resources AH-GP1-[color]-H Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 67.6 MPa | 9800 psi | ASTM D638 |
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 67.6 MPa | 9800 psi | ASTM D638 |
Polymer Resources AH-GP2-[color]-H Acetal Homopolymer, Medium Flow, General Purpose Molding, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 67.6 MPa | 9800 psi | ASTM D638 |
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 67.6 MPa | 9800 psi | ASTM D638 |
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 67.6 - 141 MPa | 9800 - 20500 psi | Average value: 98.2 MPa Grade Count:17 |
Overview of materials for ABS/Polyester Alloy + GF This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro.. |
|||
Tensile Strength, Yield | 67.6 MPa | 9800 psi | ASTM D638 |
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 67.6 MPa | 9800 psi | ASTM D638 |
Global GPP-240C 40% Glass Reinforced, Chemically Coupled Impact Polypropylene Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 67.6 MPa | 9800 psi | ASTM D638 |
Techmer ES Luriblend® HTN 05007 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, High Heat Resistance and LubricatedAppearance: BlackInformation provided by TP Composites, .. |
|||
Tensile Strength, Yield | 67.6 MPa | 9800 psi | ASTM D638 |
PlastxWorld CEVIAN® EG506 ABS Inherently Static Dissipative and Glass Fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plastx.. |
|||
Tensile Strength, Yield | 67.6 MPa | 9800 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 3501 GF-20 Description: Reinforced Grade, 20%Glass FilledInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 67.6 MPa | 9800 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-20FG-0753 20% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 67.6 MPa | 9800 psi | ASTM D638 |
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength
(Unverified Data**) Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 67.6 MPa | 9800 psi | ASTM D638 |
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, General Purpose Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 67.6 MPa | 9800 psi | ASTM 638 |
PlastxWorld CEVIAN® B5522 10% GF PBT/ABS Alloy Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |