Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.21 MPa | 321 psi | at 200%, no post cure; ASTM D412 |
Multibase C6-350 LH Parts A and B Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 2.21 MPa | 320 psi | 100%; ASTM D412 |
Teknor Apex Flexalloy® 3501-40-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Tensile Strength, Yield | 2.21 MPa @Strain 300 % |
320 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3630 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Tensile Strength, Yield | 2.21 MPa | 320 psi | AVG Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 5861 Fluoro-silicone Fluoro-silicone meeting MIL-R-25988BInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 2.21 MPa | 321 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 7045 Ethylene-Propylene Rubber General service EPDM.Information provided by Seals Eastern, Inc. |