Material Notes:
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppearance-ClearInformation provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
15 seconds; ASTM D2240
Tensile Strength, Yield 2.21 MPa
320 psi
100%; ASTM D412
6.07 MPa
880 psi
3; ASTM D412
7.72 MPa
1120 psi
ASTM D412
Elongation at Break 370 %
370 %
ASTM D412
Tear Strength Test 115
115
in psi, Die C; ASTM D624
Compression Set 13 %
13 %
73°F, 22 hr.; ASTM D395
54 %
54 %
158°F, 22 hr.; ASTM D395
67 %
67 %
212°F, 22 hr.; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -57.0 °C
-70.6 °F
ASTM D746