Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 - 184 MPa
10200 - 26700 psi
Average value: 121 MPa Grade Count:13
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..