Polymer Property : Tensile Strength, Yield = 179 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 83.0 - 179 MPa
12000 - 26000 psi
Average value: 101 MPa Grade Count:6
Overview of materials for Nylon 66, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate..
Tensile Strength, Yield 118 - 179 MPa
17100 - 26000 psi
Average value: 153 MPa Grade Count:4
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values..
Tensile Strength, Yield 82.7 - 179 MPa
12000 - 26000 psi
Average value: 138 MPa Grade Count:6
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma..