Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1379 - 1551 MPa | 200000 - 225000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 MH10, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Tensile Strength, Yield | >= 1379 MPa | >= 200000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 1/2 Hard, 1.5 hr at 950°F Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 1.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation.. |
|||
Tensile Strength, Yield | 1379 MPa @Strain 0.200 % |
200000 psi @Strain 0.200 % |
|
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition TH 1050 AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala.. |
|||
Tensile Strength, Yield | 1379 MPa @Strain 0.200 % |
200000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® D6AC UNS K24728 Specialty Steel Uses: High performance aircraft structural parts.Property values are for samples in the metallurgical condition: 1550°F Q + 1000°F T.Information provided by Allvac, An Allegheny Teledyne Company. |
|||
Tensile Strength, Yield | 1379 MPa @Strain 0.200 % |
200000 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® 13-8Mo Precipitation Hardening Steel, Heat Treatment: 927°C (1700°F) + Age Data provided by Allvac.Applications: Airframe structurals, missile components, valve parts, fasteners, chemical process equipment. |
|||
Tensile Strength, Yield | 1379 MPa @Strain 0.200 % |
200000 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® 9-4-30 Specialty Steel, Heat Treatment: 899°C (1650°F) + Age Data provided by Allvac.Applications: Aircraft structural components, rocket motor cases, pressure vessels, armor applications. |
|||
Tensile Strength, Yield | 1379 MPa @Strain 0.200 % |
200000 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® D6AC Specialty Steel, Heat Treatment: 913°C (1675°F) Q+T Data provided by Allvac.Applications: High performance aircraft structural parts. |
|||
Tensile Strength, Yield | 1379 MPa @Strain 0.200 % |
200000 psi @Strain 0.200 % |
|
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 900 AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |
|||
Tensile Strength, Yield | 1379 MPa | 200000 psi | |
HP Alloys Alloy 718, 10% Cold Worked, Aged 10% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |