Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 200000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1379 - 1551 MPa
200000 - 225000 psi
Materion Beryllium Nickel Strip - Alloy 360 MH10, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..
Tensile Strength, Yield 1380 MPa
200000 psi
50% Cold Rolled
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy
MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers..
Tensile Strength, Yield >= 1379 MPa
>= 200000 psi
Materion Beryllium Nickel Strip - Alloy 360 1/2 Hard, 1.5 hr at 950°F
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 1.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation..
Tensile Strength, Yield 1380 MPa

@Strain 0.200 %
200000 psi

@Strain 0.200 %
Aged to ~ 46 HRC
Bohler-Uddeholm UDDEHOLM CORRAX® Precipitation Hardening Stainless Mold Steel
A precipitation hardening stainless steel which offers excellent high corrosion resistance, excellent dimensional stability during hardening and good wear resistance. It can be used at its as-suppli..
Tensile Strength, Yield 1379 MPa

@Strain 0.200 %
200000 psi

@Strain 0.200 %
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition TH 1050
AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala..
Tensile Strength, Yield 1380 MPa
200000 psi
R<sub>p</sub>02. short transverse direction. 48 HRC.
Assab Steels DIEVAR Hot Work Steel
DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i..
Tensile Strength, Yield 1379 MPa

@Strain 0.200 %
200000 psi

@Strain 0.200 %
ATI Allvac® Nickelvac® D6AC UNS K24728 Specialty Steel
Uses: High performance aircraft structural parts.Property values are for samples in the metallurgical condition: 1550°F Q + 1000°F T.Information provided by Allvac, An Allegheny Teledyne Company.
Tensile Strength, Yield 1379 MPa

@Strain 0.200 %
200000 psi

@Strain 0.200 %
ATI Allvac® Vasco® 13-8Mo Precipitation Hardening Steel, Heat Treatment: 927°C (1700°F) + Age
Data provided by Allvac.Applications: Airframe structurals, missile components, valve parts, fasteners, chemical process equipment.
Tensile Strength, Yield 1379 MPa

@Strain 0.200 %
200000 psi

@Strain 0.200 %
ATI Allvac® Vasco® 9-4-30 Specialty Steel, Heat Treatment: 899°C (1650°F) + Age
Data provided by Allvac.Applications: Aircraft structural components, rocket motor cases, pressure vessels, armor applications.
Tensile Strength, Yield 1379 MPa

@Strain 0.200 %
200000 psi

@Strain 0.200 %
ATI Allvac® Vasco® D6AC Specialty Steel, Heat Treatment: 913°C (1675°F) Q+T
Data provided by Allvac.Applications: High performance aircraft structural parts.
Tensile Strength, Yield 1379 MPa

@Strain 0.200 %
200000 psi

@Strain 0.200 %
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 900
AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base..
Tensile Strength, Yield 1379 MPa
200000 psi
HP Alloys Alloy 718, 10% Cold Worked, Aged
10% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int..
Copyright © lookpolymers.com All Rights Reserved