Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.38 MPa | 1360 psi | ASTM D412 |
Polymax® Maxelast® P3877 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 9.38 MPa | 1360 psi | ASTM D412 |
Polymax® Maxelast® P3880 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 9.38 MPa | 1360 psi | ASTM D412 |
Precision Polymer Engineering C70R Chloroprene Rubber Red Iron Oxide filled, Chloroprene Rubber, 66-75 °IRHD. Flame retarding.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum based oils. .. |
|||
Tensile Strength, Yield | >= 9.38 MPa | >= 1360 psi | Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7344 Highly Saturated Nitrile Rubber HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc. |