Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.0 - 135 MPa
3920 - 19600 psi
Average value: 47.0 MPa Grade Count:34
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
Tensile Strength, Yield 135 - 135 MPa

@Temperature 130 - 175 °C
19600 - 19600 psi

@Temperature 266 - 347 °F
Average value: 135 MPa Grade Count:1
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
Tensile Strength, Yield 135 - 135 MPa

@Time 1.80e+7 - 7.20e+7 sec
19600 - 19600 psi

@Time 5000 - 20000 hour
Average value: 135 MPa Grade Count:1
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
Tensile Strength, Yield 60.0 - 135 MPa
8700 - 19600 psi
Average value: 115 MPa Grade Count:12
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..