Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.900 MPa
131 psi
70°C for 1,000 hrs; JIS-K-6251(#2)
Fujipoly Industries Sarcon® GR-Fd Gap Filler Pad
Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Fd has a mesh embedded overall.Information provided b..
Tensile Strength, Yield 0.900 MPa
131 psi
60°C for 1,000 hrs with 90% RH; JIS-K-6251(#2)
Fujipoly Industries Sarcon® GR-HFd Gap Filler Pad
Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-HFd has a hardened top surface and mesh embedded over..
Tensile Strength, Yield >= 0.903 MPa
>= 131 psi
Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 7017 Ethylene-Propylene Rubber
General service EPM.Information provided by Seals Eastern, Inc.
Tensile Strength, Yield >= 0.903 MPa
>= 131 psi
Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 7017 Ethylene-Propylene Rubber
General service EPM.Information provided by Seals Eastern, Inc.