Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 0.903 MPa | >= 131 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7017 Ethylene-Propylene Rubber General service EPM.Information provided by Seals Eastern, Inc. |
|||