Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-HFd has a hardened top surface and mesh embedded overall.Information provided by Fujipoly Industries
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
60°C for 1,000 hrs with 90% RH; JIS-K-6220
2.60 g/cc
2.60 g/cc
150°C for 1,000 hrs; JIS-K-6220
2.60 g/cc
2.60 g/cc
JIS-K-6220; ASTM D-792
2.60 g/cc
2.60 g/cc
70°C for 1,000 hrs; JIS-K-6220
Mechanical Properties Metric English Comments
Hardness, Shore C 20
20
60°C for 1,000 hrs with 90% RH; SRIS0101
22
22
70°C for 1,000 hrs; SRIS0101
29
29
150°C for 1,000 hrs; SRIS0101
Hardness, Shore OO 49
49
SRIS0101; ASTM D-2240
Tensile Strength, Yield 0.500 MPa
72.5 psi
150°C for 1,000 hrs; JIS-K-6251(#2)
0.700 MPa
102 psi
JIS-K-6251(#2)/ASTM D-412
0.900 MPa
131 psi
60°C for 1,000 hrs with 90% RH; JIS-K-6251(#2)
1.50 MPa
218 psi
70°C for 1,000 hrs; JIS-K-6251(#2)
Elongation at Yield 50 %
50 %
150°C for 1,000 hrs; JIS-K-6251(#2)
50 %
50 %
60°C for 1,000 hrs with 90% RH; JIS-K-6251(#2)
50 %
50 %
70°C for 1,000 hrs; JIS-K-6251(#2)
60 %
60 %
JIS-K-6251(#2)/ASTM D-412
Tear Strength 1.00 kN/m
5.71 pli
150°C for 1,000 hrs; JIS-K-6252 (Angle)
1.00 kN/m
5.71 pli
70°C for 1,000 hrs; JIS-K-6252 (Angle)
2.00 kN/m
11.4 pli
JIS-K-6252 (Angle)/ASTM D-624
3.00 kN/m
17.1 pli
60°C for 1,000 hrs with 90% RH; JIS-K-6252 (Angle)
Thermal Properties Metric English Comments
Thermal Conductivity 1.50 W/m-K
10.4 BTU-in/hr-ft²-°F
JIS-R-2618; ASTM D2326
1.50 W/m-K
10.4 BTU-in/hr-ft²-°F
60°C for 1,000 hrs with 90% RH; JIS-R-2618
1.50 W/m-K
10.4 BTU-in/hr-ft²-°F
70°C for 1,000 hrs; JIS-R-2618
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+13 ohm-cm
8.00e+13 ohm-cm
60°C for 1,000 hrs with 90% RH; JIS-K-6249
1.00e+14 ohm-cm
1.00e+14 ohm-cm
JIS-K-6249/ASTM D257
6.80e+14 ohm-cm
6.80e+14 ohm-cm
150°C for 1,000 hrs; JIS-K-6249
9.30e+14 ohm-cm
9.30e+14 ohm-cm
70°C for 1,000 hrs; JIS-K-6249
Dielectric Strength 10.0 kV/mm
254 kV/in
JIS-K-6249; ASTM D-149
12.0 kV/mm
305 kV/in
70°C for 1,000 hrs; JIS-K-6249
13.0 kV/mm
330 kV/in
60°C for 1,000 hrs with 90% RH; JIS-K-6249
14.0 kV/mm
356 kV/in
150°C for 1,000 hrs; JIS-K-6249
Dielectric Breakdown 8000 V
8000 V
Withstand Voltage [V/min]; JIS-K-6249; ASTM D-149
Descriptive Properties Value Comments
Color Dark Grey