Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 483 - 896 MPa | 70000 - 130000 psi | |
Meehanite Ductliron® SH-100 Nodular Graphite Ductile Iron Type SP-100 is characterized by its exceptional hardenability. It is particularly suited where high strengths are desired in relatively heavy casting sections. In the as-cast condition it has a pe.. |
|||
Tensile Strength, Yield | 414 - 896 MPa @Strain 0.200 % |
60000 - 130000 psi @Strain 0.200 % |
|
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Cold-Drawn Rod and Bar specifically. Other property values are typical of annealed DURANICKEL®.. |
|||
Tensile Strength, Yield | 758 - 896 MPa @Strain 0.200 % |
110000 - 130000 psi @Strain 0.200 % |
Heat Treatment (Condition T HRc 26-32) |
Schmolz + Bickenbach 416 Stainless Steel Bar Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity.. |