Axiall 14750 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 14750 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.37 - 1.41 g/cc
1.37 - 1.41 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 72 - 78
72 - 78
delayed; ASTM D-2240
Tensile Strength, Yield 8.62 MPa
1250 psi
ASTM D-638
Elongation at Yield 240 %
240 %
ASTM D-638
100% Modulus 0.00593 GPa
0.860 ksi
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 166 °C
330 °F