Mechanical Properties Metric English Comments
Tensile Strength, Yield 620 MPa

@Strain 0.200 %
89900 psi

@Strain 0.200 %
Hogen Diemitechâ„¢ Tungsten-Based Metal
Diemitech is a new tungsten-based material used for high temperature tooling, die casting, extrusion dies, hot upsetting, and electro brazing. It has a higher tungsten content than similar available..
Tensile Strength, Yield 620 MPa

@Strain 0.200 %
89900 psi

@Strain 0.200 %
Hogen HM3050 Tungsten-Based Metal
Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; AMS T-21014 Class 3. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE..
Tensile Strength, Yield 620 - 800 MPa
89900 - 116000 psi
Materion Beryllium Copper Alloy 25 Strip; H (TD04) Temper (UNS C17200)
Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1Formability Ratio (bad Way): 2.9Superficial Hardness: 30T 79-83Tabulated properties appl..
Tensile Strength, Yield 620 - 870 MPa
89900 - 126000 psi
Materion Beryllium Copper Alloy 25 Wire; 1/2H (TD02) Temper; 1.3-12.7 mm Diameter (UNS C17200)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Yield 620 - 870 MPa
89900 - 126000 psi
Materion Beryllium Copper Alloy M25 Wire; 1/2H (TD02) Temper; 1.3-12.7 mm Diameter (UNS C17300)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Yield 620 MPa

@Strain 0.200 %
89900 psi

@Strain 0.200 %
Mi-Tech Metals Diemitechâ„¢ Tungsten-Based Metal
Diemitech is a new tungsten-based material used for high temperature tooling, die casting, extrusion dies, hot upsetting, and electro brazing. It has a higher tungsten content than similar available..
Tensile Strength, Yield 620 MPa

@Strain 0.200 %
89900 psi

@Strain 0.200 %
Mi-Tech Metals HD17BB Tungsten-Based Metal
ASTM B-777-07 Class 1; Slightly Magnetic (HD17 is non-magnetic).Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist t..
Tensile Strength, Yield 620 MPa

@Strain 0.200 %
89900 psi

@Strain 0.200 %
Mi-Tech Metals HD18D Tungsten-Based Metal
Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; ASTM B-777-07 Class 3; AMS T-21014 Class 3. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal con..
Tensile Strength, Yield 620 MPa

@Strain 0.200 %
89900 psi

@Strain 0.200 %
Haynes 214® alloy, 20% cold reduction, 980°C (1800°F) for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Yield 620 MPa

@Temperature 100 °C
89900 psi

@Temperature 212 °F
Wet; EN2561
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Information provided by HexCel
Tensile Strength, Yield 620 - 758 MPa

@Strain 0.200 %
89900 - 110000 psi

@Strain 0.200 %
Ametek AM 388™ Alloy (UNS C72650) TM02
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Tensile Strength, Yield 620 - 750 MPa
89900 - 109000 psi
ArcelorMittal Complex Phase Steel 750 Very high strength steel, Hot Rolled Steel
Available in the following: uncoated (HCT750C) and Extragal®/Galvannealed (HCT750C+Z)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) prod..
Tensile Strength, Yield 620 MPa
89900 psi
Latrobe Nitralloy® 135 Modified VAC-ARC, 1.5 to 3 in Premium Nitriding Steel
NITRALLOY 135 MODIFIED VAC-ARC steel is a low alloy nitriding grade with moderate hardenability. It has been designed to provide a high case hardness and to maintain its core strength during the nit..