Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 11.5 MPa | 1670 psi | 15% change after 70 hours @ 125°C; ASTM D412 |
Precision Polymer Engineering E50Q Ethylene Propylene Rubber Peroxide cured, Ethylene Propylene Terpolymer, 46-55 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Complies with FDA code of Federal regulations title CFR21 section 177.2600. Water .. |
|||
Tensile Strength, Yield | 11.5 MPa | 1670 psi | ASTM D412 |
Precision Polymer Engineering E80E Ethylene Propylene Rubber General Purpose, Ethylene Propylene Terpolymer (EPT) 75-85 IRHD. Terpolymer of ethylene, propylene and diene monomers. To meet Aerospace specification DTD 5597A Grade 80. ASTM & ISO designation = E.. |
|||
Tensile Strength, Yield | 11.5 MPa | 1670 psi | ASTM D412 |
Precision Polymer Engineering E80H Ethylene Propylene Rubber Sulphur cured, white Ethylene Propylene Terpolymer, 75-85 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated using only those ingredients determined by the United States Feder.. |
|||
Tensile Strength, Yield | 11.5 MPa | 1670 psi | ASTM D638 |
Reliance Industries Reclair M26500 Polyethylene High flow Linear Low Density Polyethylene grade. Reclair M26500 is a butene comonomer with optimum levels of antioxidants.Characteristics:narrow molecular weight distribution, excellent processabi.. |
|||
Tensile Strength, Yield | 11.5 MPa | 1670 psi | Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern Perflas® 9294 Perfluorinated Rubber Perfluoro rubber for aggressive chemical service. Perflas ® 9294 seals are made of a chemical resistant perfluorinated fluoroelastomer (FFKM). Perflas 9294 seals offer outstanding resistance to.. |
|||
Tensile Strength, Yield | 11.5 MPa | 1670 psi | ISO 527-2 |
Carmel Olefins IPETHENE® 830 Low Density Polyethylene IPETHENE® 830 is a low density polyethylene injection molding grade. It exhibits high melt flow rate and high stiffness. APPLICATIONS IPETHENE® 830 is used to produce lids, containers, toys, and.. |
|||
Tensile Strength, Yield | 11.5 MPa | 1670 psi | |
Radici Radilene® R 30 IE 0 3036 B Low Density Polyethylene Shore hardness: 55 D (3s)Processable, recyclable, no charge and completely non-toxicApplication examples: coating of corrugated and non-corrugated pipe (conduit, plumbing pipe, steel pipe coating a.. |
|||
Tensile Strength, Yield | 11.5 MPa | 1670 psi | ASTM D638 |
ExxonMobil Santoprene® 223-50 Thermoplastic Elastomer
(discontinued **) A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |